Achievement of Ultralow Elastic Modulus through Optimization of Phase Stability and Recrystallization Texture in Ti – Nb – Fe – Sn Alloys
Ti–Nb–Fe–Sn alloys with relatively low Nb content, located near the phase boundary of (β + ω)/β, are designed on the basis of electron-to-atom (e/a) ratio, d-electron alloy design concept, and Mo equivalent (Moeq) aiming at low Young's modulus comparable to human bone. The effect of Sn content and Nb content on the microstructure and the mechanical properties is investigated in Ti–5Nb–3Fe–(0–6)Sn (at%) and Ti–(3–9)Nb–3Fe–4Sn (at%) alloys. The composition dependence of Young's modulus and tensile strength of Ti–Nb–Fe–Sn alloys is analyzed in terms of the phase stability, ω phase, and recrystallization texture. Both Nb and Sn are effective in suppressing the athermal ω phase and stabilizing the β phase. The recrystallization texture is strongly influenced by the content of Sn and Nb. A strong {110}β<001>β Goss texture is formed in the Ti–5Nb–3Fe–(2–4)Sn and Ti–(3–5)Nb–3Fe–4Sn alloys. The Ti–5Nb–3Fe–4Sn alloy exhibits an exceptionally low Young's modulus of 30 GPa due to the combined effects of low stability of the β phase, a small amount of ω phase, and a strong Goss texture.
Surgeons face a significant challenge due to the heat generated during drilling, as excessive temperatures at the bone-tool interface can lead to irreversible damage…
The quest for lightweight, high-performance structural materials for demanding applications such as in the fields of automotive, aerospace, and other high-tech and military industries pushes the…
Falling on the ground can cause serious injuries such as bruises, broken bones, head injuries, etc. Annually, 684,000 individuals die globally fromfalling to the ground. There are more than 37…